ITW Performance Polymers
ITW Performance Polymers Adhesives, Encapsulation & Industrial Repair Solutions
ITW Performance Polymers develops structural and semi-structural adhesives, potting and encapsulation compounds, industrial repair materials, protective polymer coatings, and epoxy grouting and chocking systems. Relevant technology platforms include Plexus® structural adhesives, Insulcast® electrical and electronic encapsulation materials, Devcon® repair and maintenance compounds, and Chockfast® and Epocast® grouting and chocking solutions for demanding industrial assemblies and equipment.
As an authorized ITW Performance Polymers distributor, Krayden supports customers evaluating materials for bonding, electrical protection, equipment repair, wear protection, and machinery foundation applications. Our team can help compare chemistries, substrates, processing requirements, application conditions, and other product-specific selection factors before a material is specified.
Markets Served by ITW Performance Polymers
Featured ITW Performance Polymers Brands
Key technology platforms relevant to structural bonding, electrical encapsulation, industrial repair, and machinery grouting and chocking.
Plexus®
Structural and semi-structural adhesive technologies for bonding composites, thermoplastics, metals, and mixed-material assemblies across manufacturing applications.
Insulcast®
Epoxy and silicone potting and encapsulation compounds for electrical and electronic assemblies, including general-purpose and thermal-management applications.
Devcon®
Industrial repair, rebuilding, wear-protection, corrosion-control, and adhesive technologies for OEM and maintenance applications.
Chockfast®
Epoxy grouting and chocking systems used to support alignment, foundation, and machinery-installation requirements in industrial and marine environments.
Epocast®
Chocking compounds and related materials associated with machinery mounting and marine equipment-installation applications.
Structural Adhesives
ITW Performance Polymers supports structural bonding through Plexus methacrylate and polyurethane technologies and Devcon epoxy adhesive systems. These materials are used across composite, thermoplastic, metal, and mixed-material assemblies where the adhesive must be selected around substrate condition, bondline geometry, working time, fixturing, production method, and the mechanical and environmental demands of the finished assembly.
Potting and Encapsulation Compounds
Insulcast epoxy and silicone compounds are used to pot, cast, and encapsulate electrical and electronic assemblies where protection, insulation, thermal management, flow, flexibility, or production processing requirements influence material choice. Applications include printed circuit boards, power supplies, transformers, batteries, ignition components, and other electrical equipment; the appropriate chemistry depends on the assembly design and product-specific electrical, thermal, mechanical, and processing requirements.
Repair Compounds and Protective Coatings
Devcon repair compounds and coating technologies are used to rebuild damaged surfaces, repair metal or rubber components, and protect industrial equipment against wear, abrasion, corrosion, erosion, and related maintenance challenges. Choosing the right material depends on the base substrate, damage mechanism, application thickness, surface preparation, equipment geometry, cure window, and the mechanical, chemical, or wear conditions expected in service.
Epoxy Grouts and Chocking Compounds
ITW Performance Polymers supplies epoxy grouting and chocking technologies for machinery foundations, alignment, mounting, and load-transfer applications. Chockfast systems span industrial grouting and chocking, while Epocast products are associated with machinery and marine chocking. Material selection and installation should be based on equipment type, load path, foundation condition, placement geometry, grout or chock dimensions, application temperature, and the product-specific installation procedure.
Talk to our Experts
Krayden can help compare ITW Performance Polymers materials for structural bonding, potting and encapsulation, industrial repair and protection, and machinery grouting or chocking. Our team can support product selection, substrate and application requirements, processing considerations, and comparison of candidate materials for your assembly or maintenance application.
ITW Performance Polymers Quick Reference
42 products

ITW PLEXUS MA422
- 10:1 Controlled Mixing
- 17 to 20-Minute Working Window
- 0.75 to 9.5 mm Gap Range

ITW PLEXUS MA832
- 10:1 Controlled Mixing
- 12 to 14-Minute Working Window
- Glass-Bead Bondline Control

DEVCON FLEXANE 94
- 6,000 cP Castable Urethane
- Replacement-Part and Flexible-Mold Fabrication
- 19.3 MPa Cured Tensile Strength

INSULCURE 11B
- Heat-Curing INSULCAST Epoxy Curing Agent
- 700 cP Application Viscosity
- 3-Hour 100 deg C Cure

DEVCON SF5MIN
- Fast Five-Minute Metal Repair
- Non-Sag Vertical Rebuilding
- Machinable Steel-Filled Repairs

PLEXUS AO420
- Controlled 4-6 Minute Assembly
- Broad 0.75-9.5 mm Gap Range
- Balanced Strength and Elongation

PLEXUS MA1020
- Very Low Cure Shrinkage
- Fast 15-20 Minute Strength Build
- Broad 0.75-9.5 mm Gap Range

PLEXUS MA2045
- Extended 45-50 Minute Work Window
- Vertical Non-Sag Placement
- Deep 38 mm Gap Bonding

PLEXUS MA300/3000
- Simple 1:1 Meter-Mix Processing
- Fast 3-6 Minute Assembly
- High-Strength Stiff Cured Bond

PLEXUS MA320
- Controlled 10-11 Minute Assembly
- Broad 0.75-9.5 mm Gap Range
- Flexible 40-80% Cured Elongation

PLEXUS MA420FS
- Rapid 1-2 Minute Work Window
- Controlled 1-4 mm Gap Range
- Robotic Plastic Assembly Fit

PLEXUS MA420W
- Fast 3-4 Minute Assembly
- Rapid 13.5-Minute Strength Build
- Wide 0.25-9.5 mm Gap Range

PLEXUS MA425
- 30-35 Minute Working Time
- Non-Sag Thixotropic Dispensing
- 30-50% Typical Elongation

PLEXUS MA440
- Self-Leveling Two-Part System
- 15 MPa Typical Tensile Strength
- 121 deg C Air Service Limit

PLEXUS MA530
- 30-40 Minute Working Time
- Up to 18 mm Gap Tolerance
- 90-160% Typical Elongation

PLEXUS MA590
- 90-105 Minute Working Time
- Up to 38.1 mm Gap Fill
- >130% Typical Elongation

PLEXUS MA8105
- Primerless Multi-Material Bonding
- Easy 1:1 Mixing
- Low-Odor Non-Filled Formulation

PLEXUS MA8120
- Low-Halogen Primerless System
- Broad Coated-Metal Adhesion
- Salt-Spray Environmental Resistance

PLEXUS MA830
- 4-6 Minute Working Time
- Fast Primerless Metal Assembly
- 2,610-3,190 psi Tensile Strength

PLEXUS MA920
- Fast 4-6 Minute Working Window
- Low-Odor Structural Bonding
- Balanced Strength and Elongation

Plexus® MA8110 | Two-Part Methacrylate Adhesive
- 1:1 Controlled Mixing
- 9 to 11-Minute Working Window
- 24.8 MPa Cured Tensile Strength

Plexus® MA1130 | Two-Part Methacrylate Adhesive
- Two-part methacrylate for multi-material structural bonding
- 26–33 minute work time at 75°F
- Gap tolerance up to 0.5 inch

PERMATEX 2BR
- Slow-Drying Gasket Dressing
- Controlled Tacky Assembly
- Fluid- and Heat-Resistant Sealing

DEVCON FL-20
- 30 to 120-Minute Moisture Cure
- Multi-Substrate Flexane Adhesion Promotion
- One-Part No-Mix Primer

ARALDITE CW 177
- Mineral-Filled Electrical Casting Epoxy
- 22,000 to 27,000 mPa s Casting Viscosity
- Transformer and Capacitor Encapsulation

INSULCAST RTVS A-4000
- Two-Component Solvent-Based Silicone Adhesive for Silicones
- 900 to 2,500 cP Mixed Viscosity
- 73 to 260 deg C Service Range

INSULCAST RTVS 8128
- Low-Viscosity Encapsulation Application
- 2,200 cP Mixed Viscosity
- 55 to 204 deg C Service Range

DEVCON 10 MINUTE EPOXY
- 10-Minute Working Window
- 1:1 Meter-Mix Processing
- 31.5 kV/mm Dielectric Strength

DEVCON 10760
- Titanium-Reinforced Epoxy Putty
- Non-Sag Placement Control
- Machinery Repair Applications

DEVCON PLASTIC STEEL
- Room-Temperature Adhesive Cure
- 45-Minute Working Window
- 2,800 psi Cured Tensile Strength

DEVCON PLASTIC WELDER
- Steel-to-Wood Methacrylate Bonding
- 3-Minute Open Time
- 20.6 MPa Cured Tensile Strength

PLEXUS MA330
- Extended 15-18 Minute Work Window
- Defined 30-45 Minute Fixture
- High-Strength 1:1 Structural Bonding

PLEXUS PC-120
- Visible Red Application Indicator
- Fast 1-3 Minute Bonding Window
- Brush or Wipe Metal Conditioning

INSULGEL 70 CC
- Low-Shrinkage Thermal-Shock-Resistant Epoxy
- Three Curing-Agent Options
- Shore D 43 to 80 Hardness

DEVCON FLEXANE 80
- Medium-Viscosity Application Control
- 10-Hour Cure Cycle
- Shore A 87 and 650% Elongation

INSULCAST 116 FR-FC
- Equal-Ratio Production-Line Epoxy Potting
- 9,800 cP Mixed Viscosity
- UL 94 V-0 Classification

INSULCAST 140 FR
- Epoxy Casting with Insulcure 11B
- 50,000 cP Mixed Viscosity
- 2.3 W/(m K) Thermal Encapsulation

INSULCAST 502
- Low-Viscosity Encapsulation Application
- Room-Temperature Encapsulation Cure
- 200 to 300 cP Mixed Viscosity

INSULCAST 987
- Semi-Flexible Broad-Temperature Epoxy Potting
- 60,000 cP Mixed Viscosity
- -55 to 155 deg C Service Range

INSULCAST RTVS 8127
- Flame-Retardant 1:1 Silicone Encapsulation
- 4,000 cP Mixed Viscosity
- 0.75 W/(m K) Thermal Encapsulation

RTVS 3-95-2
- 1:1 weight or volume mix
- 1.44 W/(m K) thermal conductivity
- -55 to 260 deg C service range

PLEXUS H4110
- Extended 8-12 Minute Work Window
- Non-Sag Gel Placement
- Elastic Mixed-Material Bonding