TIP 1500 | Thermal insulator pad

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TIP1500 | Thermal insulator pad

Main features

  • 0.54 - 0.61 Thermal Impedance
  • 1.5 Thermal Conductivity
  • 0.23mm Thickness

Product Description

Honeywell's TIP1500 thermal insulator pad is designed to provide low thermal impedance and high isolation for high power and high voltage applications. Integrated fiberglass reinforcement protects the pad from tears, cut-throughs and punctures.It is designed to be soft and conformal which provides excellent mating surface for low pressure mounting.

TIP1500 comes in a pink color and offers 0.19mm and 0.23mm thickness. While the Breakdown voltage between TIP 1500 and TIP 3500 is identical and they are both V0 rated, their dielectric properties differ, mostly as an effect of the different thicknesses. Please consult the Specification fields and the Technical data sheets for additional information

Product Family

SOLSTICE TIP1500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Pink
Film ThicknessFilm Thickness
0.19 - 0.22 mm
Specific GravitySpecific Gravity
2.21
Thermal Properties
Thermal ConductivityThermal Conductivity
1.5 W/m.K
Thermal ImpedanceThermal Impedance
0.54 - 0.61 °C·cm²/W
UL 94 RatingUL 94 Rating
V-0
Electrical Properties
Breakdown VoltageBreakdown Voltage
>6000 V
Volume ResistivityVolume Resistivity
10000000000000 Ohms⋅cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers